"Sarrafa ma'auni ta cikakkun bayanai, nuna tauri ta inganci". Kamfaninmu ya yi ƙoƙari ya kafa ma'aikata masu inganci da kwanciyar hankali kuma sun bincika ingantaccen tsarin gudanarwa mai inganci don Mafi ƙarancin Farashi donChina Ferrite Magnets Fayil don Fara Babur, Muna fatan gaske don tantance wasu gamsassun hulɗa tare da ku a cikin kusancin dogon lokaci. Za mu sanar da ku ci gaban da muka samu kuma mu tsaya tsayin daka don gina ci gaban ƙananan kasuwanci tare da ku.
"Sarrafa ma'auni ta cikakkun bayanai, nuna tauri ta inganci". Kamfaninmu ya yi ƙoƙari ya kafa ma'aikata masu inganci da kwanciyar hankali da kuma bincika ingantaccen tsarin gudanarwa mai inganci donChina Ferrite,Abubuwan Motoci, Mun hade zane, yi da kuma fitarwa tare da fiye da 100 gwani ma'aikata, m ingancin kula da tsarin da gogaggen technology.We ci gaba da dogon lokaci kasuwanci dangantaka da wholesaler da masu rarraba kafa fiye da 50 kasashen, kamar Amurka, UK, Canada, Turai da kuma Afirka da dai sauransu.
Gabatarwa:
Maganganun SmCo suna wakiltar sabbin ƙarni na kayan maganadisu. An haɓaka su sama da shekaru 40 da suka gabata kuma sun gabatar da zamanin dindindin na injin maganadisu. A wancan lokacin, wadannan karafa da ba kasafai suke yi ba suna da tsada sosai. A cikin 1980s, SmCo abu ya ƙara maye gurbinsa da NdFeB maganadiso. Sakamakon hauhawar farashin mai ban mamaki a cikin duniyar neodymium da dysprosium (Nd/Dy), wannan abu yanzu ya dawo da shahararsa a aikace-aikace a yanayin zafi mai girma (150°C – 200°C). Koyaya, akwai iyakoki da aka saita akan kayan dangane da matsakaicin kasancewarsa. Manyan nau'ikan maganadisu na SmCo guda biyu suna samuwa, nau'in 1:5 (SmCo5) da nau'in 2:17 (Sm2Co17). SmCo maganadiso suna da super high Magnetic Properties da zazzabi Properties.
Amfani:
Amfani da waɗannan maganadiso yana da yanayin zafin jiki a cikin kewayon da ke gudana daga 250ºC zuwa 350ºC kuma zafin su na Curie zai iya kaiwa 710 zuwa 880 ° C. Saboda haka, SmCo maganadisu yana da mafi kyaun magnetic kwanciyar hankali saboda m juriya ga high zafin jiki. SmCo maganadiso suna halin sosai high lalata juriya, babu shafi da ake bukata domin surface kariya.
Siffa:
Rashin lahani na maganadisu na SmCo shine alamar rashin ƙarfi na kayan - al'amari wanda dole ne a yi la'akari da shi musamman yayin sarrafawa. Abubuwan maganadisu suna galvanized ko rufaffiyar ta hanyar electrodeposition cathodic don wasu aikace-aikace.
Aikace-aikace:
A cikin wuraren da yawan zafin jiki na aiki, babban lalata da juriya na iskar shaka suna da mahimmanci. Kamar Electronic magnetron, Magnetic watsa, Magnetic magani, Magnistor, da dai sauransu.
An ƙaddara duk ƙimar da aka bayyana ta amfani da daidaitattun samfuran bisa ga IEC 60404-5. Abubuwan dalla-dalla masu zuwa suna aiki azaman ƙimar tunani kuma suna iya bambanta. Max. zafin aiki shine
ya dogara da girman maganadisu da takamaiman aikace-aikacen. Don ƙarin bayani don Allah
tuntuɓi injiniyoyinmu na aikace-aikacen.
Sintered SmCo Magnet Abubuwan Jiki | |||||||||
Kayan abu | Daraja | Kasancewa | Rev. Temp.- Coeff. Daga Br | Karfin Tilastawa | Ƙarfin Ƙarfin Ƙarfi na ciki | Rev. Temp.-Coeff. da Hcj | Max. Samfuran Makamashi | Max. Yanayin Aiki | Yawan yawa |
Br (KGs) | Hcb (KA) | Hcj (KA) | (BH) max. (MGOe) | g/cm³ | |||||
SmCo5 | XG16 | 8.1-8.5 | -0.050 | 7.8-8.3 | 15-23 | -0.30 | 14-16 | 250 ℃ | 8.3 |
XG18 | 8.5-9.0 | -0.050 | 8.3-8.8 | 15-23 | -0.30 | 16-18 | 250 ℃ | 8.3 | |
XG20 | 9.0-9.4 | -0.050 | 8.5-9.1 | 15-23 | -0.30 | 19-21 | 250 ℃ | 8.3 | |
XG22 | 9.2-9.6 | -0.050 | 8.9-9.4 | 15-23 | -0.30 | 20-22 | 250 ℃ | 8.3 | |
XG24 | 9.6-10.0 | -0.050 | 9.2-9.7 | 15-23 | -0.30 | 22-24 | 250 ℃ | 8.3 | |
XG16S | 7.9-8.4 | -0.050 | 7.7-8.3 | ≥23 | -0.28 | 15-17 | 250 ℃ | 8.3 | |
XG18S | 8.4-8.9 | -0.050 | 8.1-8.7 | ≥23 | -0.28 | 17-19 | 250 ℃ | 8.3 | |
XG20S | 8.9-9.3 | -0.050 | 8.6-9.2 | ≥23 | -0.28 | 19-21 | 250 ℃ | 8.3 | |
XG22S | 9.2-9.6 | -0.050 | 8.9-9.5 | ≥23 | -0.28 | 21-23 | 250 ℃ | 8.3 | |
XG24S | 9.6-10.0 | -0.050 | 9.3-9.9 | ≥23 | -0.28 | 23-25 | 250 ℃ | 8.3 | |
Sm2Co17 | Saukewa: XG24H | 9.5-10.2 | -0.025 | 8.7-9.6 | ≥25 | -0.20 | 22-24 | 350 ℃ | 8.3 |
XG26H | 10.2-10.5 | -0.030 | 9.4-10.0 | ≥25 | -0.20 | 24-26 | 350 ℃ | 8.3 | |
XG28H | 10.3-10.8 | -0.035 | 9.5-10.2 | ≥25 | -0.20 | 26-28 | 350 ℃ | 8.3 | |
Saukewa: XG30H | 10.8-11.0 | -0.035 | 9.9-10.5 | ≥25 | -0.20 | 28-30 | 350 ℃ | 8.3 | |
Saukewa: XG32H | 11.0-11.3 | -0.035 | 10.2-10.8 | ≥25 | -0.20 | 29-32 | 350 ℃ | 8.3 | |
XG22 | 9.3-9.7 | -0.020 | 8.5-9.3 | ≥18 | -0.20 | 20-23 | 300 ℃ | 8.3 | |
XG24 | 9.5-10.2 | -0.025 | 8.7-9.6 | ≥18 | -0.20 | 22-24 | 300 ℃ | 8.3 | |
XG26 | 10.2-10.5 | -0.030 | 9.4-10.0 | ≥18 | -0.20 | 24-26 | 300 ℃ | 8.3 | |
XG28 | 10.3-10.8 | -0.035 | 9.5-10.2 | ≥18 | -0.20 | 26-28 | 300 ℃ | 8.3 | |
XG30 | 10.8-11.0 | -0.035 | 9.9-10.5 | ≥18 | -0.20 | 28-30 | 300 ℃ | 8.3 | |
XG32 | 11.0-11.3 | -0.035 | 10.2-10.8 | ≥18 | -0.20 | 29-32 | 300 ℃ | 8.3 | |
XG26M | 10.2-10.5 | -0.035 | 8.5-9.8 | 12-18 | -0.20 | 24-26 | 300 ℃ | 8.3 | |
XG28M | 10.3-10.8 | -0.035 | 8.5-10.0 | 12-18 | -0.20 | 26-28 | 300 ℃ | 8.3 | |
XG30M | 10.8-11.0 | -0.035 | 8.5-10.5 | 12-18 | -0.20 | 28-30 | 300 ℃ | 8.3 | |
XG32M | 11.0-11.3 | -0.035 | 8.5-10.7 | 12-18 | -0.20 | 29-32 | 300 ℃ | 8.3 | |
Saukewa: XG24L | 9.5-10.2 | -0.025 | 6.8-9.0 | 8-12 | -0.20 | 22-24 | 250 ℃ | 8.3 | |
Saukewa: XG26L | 10.2-10.5 | -0.035 | 6.8-9.4 | 8-12 | -0.20 | 24-26 | 250 ℃ | 8.3 | |
Saukewa: XG28L | 10.3-10.8 | -0.035 | 6.8-9.6 | 8-12 | -0.20 | 26-28 | 250 ℃ | 8.3 | |
Saukewa: XG30L | 10.8-11.5 | -0.035 | 6.8-10.0 | 8-12 | -0.20 | 28-30 | 250 ℃ | 8.3 | |
Saukewa: XG32L | 11.0-11.5 | -0.035 | 6.8-10.2 | 8-12 | -0.20 | 29-32 | 250 ℃ | 8.3 | |
Lura: |